PF
Thickness Required = ((W/2) x tan a) / "C"
CON-SERV Inc recommends an 11 ga. plate be laminated every 2" in pads over 2" thick for strength and stability.
Physical Properties:
Item # |
Element |
Max. Design Pressure (psi) |
Durometer (Shore A) |
Max. Compressive Strength (psi) |
Quantity |
---|---|---|---|---|---|
03SS 13CS | N/A Upper | N/A 1500 | N/A 90 | N/A 18000 | |
06CSB 25PF | N/A Lower | N/A 1500 | N/A 90 | N/A 18000 | |
06CSB 50PF | N/A Lower | N/A 1500 | N/A 90 | N/A 18000 | |
06CSB 75PF | N/A Lower | N/A 1500 | N/A 90 | N/A 18000 | |
06CSB 100PF | N/A Lower | N/A 1500 | N/A 90 | N/A 18000 | |
06CSB 125PF | N/A Lower | N/A 1500 | N/A 90 | N/A 18000 | |
06CSB 25PF 13CS 50L | N/A Alternate Lower | N/A 1500 | N/A 90 | N/A 18000 |